Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced N2U40G7 LS BK23300  - PPA-GF35 - BASF

Material Data Center offers the following functions for Ultramid® Advanced N2U40G7 LS BK23300 :
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 25 / * cm³/10min ISO 1133
Temperature 325 / * °C -
Load 2.16 / * kg -
Molding shrinkage, parallel 0.2 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.8 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 12500 / - MPa ISO 527
Stress at break 150 / - MPa ISO 527
Strain at break 2 / - % ISO 527
Flexural modulus, 23°C 12200 / - MPa ISO 178
Flexural strength 230 / - MPa ISO 178
Charpy impact strength, +23°C 60 / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 13 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 305 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 275 / * °C ISO 75-1/-2
Coeff. of linear therm. expansion, parallel 14 / * E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion, normal 62 / * E-6/K ISO 11359-1/-2
Burning behav. at thickness h V-0 / * class IEC 60695-11-10
Thickness tested 0.2 / * mm -
Other propertiesdry / condUnitTest Standard
Density 1490 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
Material specific propertiesdry / condUnitTest Standard
ISO Data
Viscosity number 70 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection MoldingValueUnitTest Standard
Melt temperature 310 - 340 °C -
Mold temperature 100 - 160 °C -
Processing Recommendation ExtrusionValueUnitTest Standard
Melt temperature 310 - 340 °C -
Characteristics
Processing
Injection Molding, Other Extrusion
Delivery form
Pellets, Black
Special Characteristics
Flame retardant, Halogen-free, Heat stabilized or stable to heat
Features
Color Stability
Applications
IT / Business Machine, Electrical and Electronical
Regional Availability
Asia Pacific
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.